this post was submitted on 15 Jun 2023
21 points (95.7% liked)

3DPrinting

15655 readers
63 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

I have spent weeks of tuning PETG to print on my modified CR-10. I would get regular failures and really stringy prints. I had trouble getting it to stick to the bed, and could only print really slowly.

I was dreading trying ASA, but I bought a roll of Polylite ASA, put it on the printer without drying it, and used a default ASA profile I found online (I didn't even start with a temp tower). The only changes I made was a minimum layer fan of 10% as my PETG fan shroud needs constant cooling. I didn't see anything about enclosure temperature so I left it at 40°.

The first print started great but broke off the bed. The Z height was off and I didn't get it fixed until the first layer was halfway done. This benchy is the second print using a default ASA profile, no tuning.

I feel like I've wasted my time with PETG. This material has been so much easier to print.

Edit: not sure why my image didn't upload. I'm new to Jerboa.

you are viewing a single comment's thread
view the rest of the comments
[–] Blackbart42 1 points 1 year ago

Looks nice, thanks for sharing. I've been meaning to try ASA for outdoor applications.