this post was submitted on 11 Nov 2024
84 points (96.7% liked)

3DPrinting

15752 readers
161 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

This was an ornament I printed roughly 6 years ago. Being a Christmas ornament it spent most of those 6 years stored in my roof space.

Being in Australia this would have been subject to average temperatures of 30 to 35 degrees c but also peaks across summer approaching 70 degrees c. Also in high humidity.

The PLA crumbles into tiny pieces at the softest touch.

I thought it was interesting that PLA would start to break down in these conditions.

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 23 points 1 month ago* (last edited 1 month ago) (1 children)

PLA is widely used as a medical plastic and its normal decomposition is into lactic acid.

Even if it is just being atomized down into smaller and smaller particles it's safer for you than any other common plastic.

The colorants added are the only risk

[–] roofuskit 19 points 1 month ago* (last edited 1 month ago)

Not entirely true as there are no industry standards for PLA. Lots of manufacturers add things they don't put on the label. Especially in the variants like PLA+ and High Speed PLA.