this post was submitted on 30 Jun 2023
6 points (100.0% liked)

3DPrinting

15261 readers
5 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I've been having some difficulty underextrusion on my new all-metal hotend. I've set my retraction distance to 1.5mm (1.0 leaves strings), but on regular PLA I'm getting occasional layers that don't print very well (particularly if there's a lot of stopping and starting), and glitter PLA is an absolute disaster.

Any suggestions for getting this to work? Does glitter PLA just not get along with all-metal hotends? Is it possible that there's hardened PLA up past the heat break that things are catching on, and if so, how can I clean that out (I've been using cleaning filament already, and it doesn't seem to be solving the issue)?

FIXED: Increasing my flow rate fixed this. I started at 110, which was a bit better, then went to 120, which was a bigger improvement, and at 125 the first layer printed perfectly.

EDIT: This was a symptom of my extruder needing to be tightened and recalibrated. It now prints perfectly with a flow rate of 100%.