this post was submitted on 05 Jul 2023
46 points (100.0% liked)

3DPrinting

15642 readers
322 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I see a lot of people claim they tune/calibrate their printer any time they use a new spool of filament. But does anyone actually do this? It feels like a waste of time when filament is so consistent, even between brands. I can understand doing it for specialty rolls, but for basic pla? Seems unnecessary

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 3 points 1 year ago* (last edited 1 year ago) (1 children)

I had the same problem with my CR-10. The issue was that the weak original bed springs were too weak to hold the bed. The vibrations of the printer allowed it to move, causing the first layer to not adhere very well. I also had filaments get moisture after a week or two.

When people say upgrade the Creality bed springs, they aren't kidding. PLA is forgiving enough on the first layer, but upgrading those bedsprings was necessary for me to print PETG. I made them stiffer by adding 5-6x washers on each post to pre-compress the springs. This makes them much stiffer and stay put.

I also bought a filament dryer. I put a new roll of PETG in the dryer and put it in continuous mode at 55°, and print PETG directly from the dryer.

I still have to print PETG pretty slowly compared to PLA or ASA (my favorite material).

To OP's original question: I do a full tuning of PETG with a new maker/roll. PETG is a co-polymer. Each manufacturer could have a different amount of glycol on the PET chain, or even a different distribution (e.g. ABABABAB copolymers behave differently than AAAABBBB copolymers even though both are 50% B). Colorants can also affect behavior.

PLA I really don't tune. I add 5-10 degrees when I'm printing quickly. That's about it. I recently was printing a spacer out of the last bit of a PLA+ roll I had. The filament ran out and the printer halted. I loaded a matte PLA to finish (I slowed the printer down and bumped the temp up manually by 5 degrees since this matte stuff has layer adhesion issues), and it also ran out before the print was done. So I loaded a roll of transparent PLA that I bought 9-10 years ago (and was stored in an attic for 2 years) and is very brittle, and it printed just fine. The print looks strange (tan to matte terra cotta to transparent purple) but works great.

[–] Sumeron 1 points 1 year ago (1 children)

Oh thanks for pointing out the bed springs! That does sound like something that can be happening, since they seem to slowly 'unwind' causing the bed to lower. I'll add some washers; thanks for the tip!

[–] [email protected] 1 points 1 year ago

I did this more as a temporary fix. There are lots of sellers of stiffer spring sets or silicone spacers for Creality printers online. There are also several models on thingiverse for printing your own spacers.