this post was submitted on 02 Jul 2023
36 points (100.0% liked)

3DPrinting

15178 readers
122 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Flashforge creator pro 2 with PLA, standard quality preset, textured removable magnetic bed on the build plate.

The first lines are straight, but as it makes more parallel lines to build the layer, it starts to develop a scalloped pattern. This creates issues with smoothness when it fills back to join it from the other side later. I've leveled the build plate, although I suspect it's not perfectly flat and maybe slightly higher in the middle. Is this my problem? It appears to have the pattern even away from the middle if that makes sense.

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 0 points 1 year ago

That's not very underextruded on the edges, and doesn't seem indicative of bed warping IMO.

Which slicer are you using? If you're using PrusaSlicer the setting you're looking for is under Advanced > Extrusion Width > External Perimeter

Other slicers will also have this option just might be called something else.

Bump that up by .02mm or so and you'll probably be golden.

For reference on a 0.4mm nozzle my external extrusion width is 0.45 for external perimeters.

You might also need to bump up the infill/perimeters overlap coefficient by a few percent.