this post was submitted on 13 Dec 2023
19 points (91.3% liked)

3DPrinting

15657 readers
129 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

How long do you have filament sitting "in the open"? I mostly print with a single filament roll at a time, and just leave it on the printer. A 1kg roll lasts me several weeks. For long time storage I keep it in an air tight box with disiccant pouches.

But how long can I let it sit before I should start storing it with disiccant and/or drying the filament before use?

you are viewing a single comment's thread
view the rest of the comments
[–] dual_sport_dork 1 points 11 months ago

I store my open but not currently used rolls of filament in a large plastic tote with a gasketed lid. I guess you could call this a "dry box," but it's not very heavy duty. I have a stocking full of silica gel desiccant beads in it, the kind that change color when they're allegedly saturated. I nuke that in the microwave about once every six months. They're never indicating their saturated color by then, but it pays to be sure.

Whatever roll is currently loaded in the printer I have in a heated filament dryer which can output right to the printer. Its lid is not sealed, per se, but it's not just open to the air, either. I run the dryer when I'm printing. That hasn't given me any issues.

In my environment -- a basement that's not terribly damp, and I leave a dehumidifier running maintaining an alleged 30% RH -- if I leave an exposed roll of PLA on the machine it will get brittle enough to potentially start snapping bits off within about 2-3 weeks of sitting exposed to open air.