I apologize for the links below being vendor specific, but the linked products are the specific products I have used. I have no affiliation with the shop other than they offer to bill my job instead of having me pay upfront and then get the expenses redeemed. (I have tried making this both subscript and super script with respectively ^ and ~, but none works on lemmy)
I seek advice on proceeding with the setup and acquiring an acceptable printing quality.
Background
I have recently "upgraded" a creality cr6 se at work. I installed a spider steel/PEI plate (https://3deksperten.dk/products/spiderflexiplate-double-system-255x245-ex-cr-6-se), a bimetal heatbreak https://3deksperten.dk/products/3dsupreme-titanium-alloy-bi-metal-heatbreak-cr6-se) and a hardened steel nozzle (0.4mm from this kit https://3deksperten.dk/products/creality-3d-3d-printing-up-market-nozzle-kit-8-pcs)
Findings
Testing this new setup I used the PLA spool I had been printing with days before without issue. The new and old nozzles are all 0.4mm.
What I discovered was that I couldn't get any adhesion to the built plate, some spray glue (this exact make and model https://3deksperten.dk/products/printafix-100ml) fixed that. Then layer adhesion was an issue. So I upped the temp to the max for this PLA and increased the extrusion rate. First 10 layers or so were somewhat ok, but the rest delaminated instantly.
I then opened a brand new spool of PLA, thinking that the old spool had moisture issues. Cranked the temp to max, 210°C, added 5°C to the bed and applied a strong shot of spray glue. This time the print actually got done, but the parts where Cura's tree support was supposed to be supporting, the layers seem to come apart. The rest of the print was somewhat ok, though not great.
Current considerations
- Maybe I attempted too much at the same time. I may try swapping the nozzle back and only deal with the plate and heatbreak.
- The heat break may be install wrong. The nozzle was screwed in all the way, loosened a few turns, then the heat break was screwed in all the way. The nozzled was then tightened. No heating was done. I may try giving the heat break a few turns before installing the old nozzle again.
- Should I have heated hotend before tightening the nozzle?
New Lemmy Post: Issues with layer adhesion post bimetal heatbreak and hardened steel nozzle install. (https://lemmy.world/post/9179879)