this post was submitted on 16 Nov 2023
49 points (98.0% liked)

3DPrinting

15254 readers
35 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Printing here with eSun PLA at 215 C on a Prusa Mini, and there are lots of hairline strings.

What's causing those strings? Temp too low?

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 8 points 10 months ago

Try dehydrateding your pla first. Then try some of these other suggestions. If all else fails, these clean up really nicely with a butane blow torch.