this post was submitted on 06 Nov 2023
33 points (94.6% liked)

3DPrinting

15596 readers
36 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
33
submitted 1 year ago* (last edited 1 year ago) by RubberElectrons to c/3dprinting
 

Hey everyone.

I built an mk3s+ from its kit form successfully, tested a few PLA prints with the stock 0.4 nozzle.

I've set prusaslicer to use a 0.6 nozzle now that I've upgraded, and am using PETG. Prints look pretty bad, in spite of calibrating z-offset etc.

If you were doing something like this for the first time, what would your setup steps be like?

To be specific, using a diamondback 0.6 nozzle, matterhackers PETG at 235c.

Issues I'm seeing are a really bad loss of detail, lots of stringing, etc.

eta: added a photo of a moderately post-processed part. Notice how rough the top surface looks, there's a disconnect between perimeter loops, etc.

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 0 points 1 year ago (1 children)

Two things I’d suggest:

Try another brand of PETG - I’ve heard weird things about MatterHackers PETG but never used it personally. Overture, Polymaker, Prusament, and Printed Solid PETG always behave consistently for me.

Take a look at your heatblock and make sure you’re not leaking anywhere. I tried a 0.8 nozzle when I first got my MK3S+ and got bad results b/c I was leaking out the top and it was stringing badly. I eventually went with a Revo nozzle because swapping is so much simpler.

[–] [email protected] 1 points 1 year ago

+1 for overture, I've had very good luck with it. That said, I'm pretty sure PETG needs to be very dry in general. Prints beautiful just out of the box, but I have terrible stringing even storing everything sealed in vacuum bags after a few prints.