this post was submitted on 11 Jul 2023
13 points (100.0% liked)

3DPrinting

15606 readers
230 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
13
Tips for PETG? (self.3dprinting)
submitted 1 year ago* (last edited 1 year ago) by WhosMansIsThis to c/3dprinting
 

Im very new to 3d printing and this is my first time using anything other than pla. So far all of my prints are lifting off the bed at the corners. They start off looking beautiful. No stringing, great adhesion, etc. But after a few layers, they start to come off. Especially on larger prints.

Heres my setup:

  • Ender 3 pro with skr mini e3 v2
  • Creality Ender 3 glass bed upgrade
  • Bed temp: 90C
  • Extruder temp: 240C
  • Nozzle diameter: .4
  • Layer height: .2
  • First layer: .45
  • Speed: 60mm/s
  • Slicer: Silc3r

I realize that asking this question is like asking WebMD to dianose my sniffles, cause it can literally be anything, but Im hoping someone with more experience can give me some pointers on what works for them. Thanks yall!

Update: First of all, thank you all so much for the kick ass suggestions! I really appreciate all of your replies. Since pretty much everyone recommended it, I went ahead and got a textured spring steel PEI plate and holy shit, it didn't disappoint. Adhesion has been fantastic. I also ended up lowering my bed temp down to 75 from 90 and pushing my hotend temp to 245 for the first layer, then back to 240. I got an enclosure to help keep the plate clean but I also stocked up on some blue dawn dish soap. I still have a little more trial and error with print speed and cooling but I'm literally getting the best prints I've ever gotten thanks to all of your suggestions. Yall are awesome and I'm really glad I posted here.

you are viewing a single comment's thread
view the rest of the comments
[–] Fubar91 3 points 1 year ago

I like to drop my cooling fan down to 10% and drop my layer hieght slightly for the first 3-5 layers of the prints for PETG. It tends to like to shift a bunch if cooled too quickly. I also have better results on a textured print surface.