Larger nozzles do kick ass. I personally use my 0.6 nozzles pretty heavily. As others have mentioned though, there are definitely scenarios where you'll really want or even need to drop to a smaller size. My printer hates trying to print PETG at higher sizes for example, maybe my hot end isn't powerful enough.
3DPrinting
3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.
The r/functionalprint community is now located at: [email protected] or [email protected]
There are CAD communities available at: [email protected] or [email protected]
Rules
-
No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.
-
Be respectful, especially when disagreeing. Everyone should feel welcome here.
-
No porn (NSFW prints are acceptable but must be marked NSFW)
-
No Ads / Spamming / Guerrilla Marketing
-
Do not create links to reddit
-
If you see an issue please flag it
-
No guns
-
No injury gore posts
If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)
Moderation policy: Light, mostly invisible
it also consumes way more filament- especially on single-wall parts or parts that have x perimeters rather than a perimeter thickness. They're great for structural prints, and large prints that you want done quickly. For comparison, a .4mm nozzle will have a nozzle area of about 0.125 mm^2, where a 0.6mm is .28 mm^2. and .8mm is .502mm^2. More than double the extrusion width.
like basically everything else in 3d printing, it's all about compromise and which compromises are acceptable.
No, I don't agree with consumes 'way more' filament.
If your design calls for 1mm width wall. You're doing two passes with a 0.4 nozzle (0.5 width x2) or one pass with a 0.8 nozzle (1 width x1)
It's the same plastic.
You'll use more plastic on the infill, but you could arguably use a lower % infill if the infill wall thickness is larger.
So you could be using more plastic overall, but I don't think it would qualify as 'way more'.. maybe like 10% to 20% more.
10-20 % comes out to $3-6 extra for the same parts across a 2kg reel. For parts that are structural or large (and not meant to be seen, or will be post processed anyway,) the advantages in strength and speed could be worth it.
But, that 3-6 adds up significantly over time.
I do agree that .6 and .8mm nozzles have a place in anyone’s kit. I don’t agree that this excludes .4mm or smaller nozzles from a similar place
It’s all about finding the right balance.
Combination of line width, layer height and speed is what limits your hottend, not the nozzle size
Wanted to reply to another comment, but its saying that language is not alliwed lol
Well, yeah.. but Line Width, Layer Height and speed are functions limited by nozzle size.
You can't make a 0.60 layer height with a 0.4 nozzle, but you can with the 0.8 nozzle.
Speed is a function of nozzle size, because you can't push 200mm/s worth of plastic through a 0.1 nozzle.
Pushing too much mass through a small nozzle creates uncontrollable back pressure.
With a large back pressure, your ability to control flow rate and die swell because too much.
Tell us about your hotend?
Pretty simple - Microswiss metal hotend with the Minimus cooling system - 2 5015 fans and all removable with no screws, it just pops right apart and I can get to the hotend in seconds. I switched the fans to JST connectors one day I'll do the same for the heater/thermistor with something like an xt30 for the heater. One day I'll get around to it
Ever try 1.0?
Ever try 1.0........
On weed?
Doctor said I need a backiotomy!
No just my first venture past 0.4
Is thicc
Goodbye, filament money! Good grief do big prints chew through supply.
3d printer go brrrrrrrrrrt
I printed some tiny but detailed board game pieces recently, I don't think I'd get the detail I wanted with a 0.8. I also have Revo installed so I'm okay with swapping nozzles frequently.
For years now, I've always want to see someone try a dual nozzle setup. Same material, same filament, but two nozzles sizes.
Small nozzle for outer perimeter at a low layer height.
Large nozzle for inner perimeter and infill at higher layer heights.
Maybe in the future, someone will find a way to control nozzle size dynamically.
Until you need to print something small and accurate that is. I had to build a second 3d printer to be able to do that even with just a 0.6mm nozzle on mine. Though I might have gone just a bit too far to the other end.
Also 0.8mm nozzles need quite the hotend to be usable. The standard Creality hotend would struggle to do 0.3mm layers at 50mm/s, and even a V6 would max out at around 0.4mm layers.
I'm not so sure about that. I have gone all-metal (and bimetallic) on my 3V2 for the, uh. The bit connecting the heater to the heat sink. The HEATBREAK. Right. But the heater block, sensor, heat sink are all original and they have absolutely no problem with 1.0mm, at least up to 220. I've done various power measurements and it's not having to work hard to do it, either.
The other changes I've made to the hot end assembly have been adding more cooling, not more heat. (It's dual fan now and has better airflow to the heatsink.)
I mean, it could all be due to the bimetallic heatbreak. But, well... 1.0mm is 100% absolutely fine on my 3V2.
So. speaking of cooling..... I've been floating an idea around for a bit now. Ever play with an airbrush kit (like for painting minis?)
hear me out here. Imagine setting up a plennum pressure chamber fed by an airbrush compressor, then using servos or something to control conic plug valves (as in the airbrush itself.) Now, imagine something similar to a bowden tube running to the hot end from said plenum chamber... directing the air exactly where you want it.
seriously, most the weight of the hot end is now in fans. At least, for me. (heater cooler, nozzle cooler, the other nozzle cooler.)
Imagine how fast we could get with bowden-air... (yeah, I'll have to work on that name...)
It's not just the nozzle size alone. Each hotend has a limit to the volumetric output, how much plastic it can melt in the time it takes the filament to travel through the hotzone in a certain time, which is roughly calculated by line_width x layer_height x print_speed, e.g 0.6 x 0.3 x 50 = 9. That the limit is varies depending on your print temperature and it also isn't linear - you start underextruding up to 50% before you hit the point where the extruders starts skipping for example - but there is a limit - for standard hotends it's usually around 15mm^(3)/s.
https://www.cnckitchen.com/blog/flow-rate-benchmarking-of-a-hotend
question... how are you dealing with extrusion pressure on the tiny nozzle? I tried going to a .2mm and found my printer didn't like the nozzle pressure. at all.
Dang, I have .8s for all my hotends but haven't got around to trying them. Some day though.
Thanks for the motivation.
When you have big shit to print try it, I've cut 20h parts down to 9h
Yeah totally get it, going to .6 already forced me to switch to 5kg spools on my commonly used filament.
Any troubles keeping up with extruding through a .8? Having a reason to spend money on a higher performance hot end was my main worry from using it.
Wow! That's awesome! What additional modifications were required?
as @rambos said, line width, layer height, and speed. I'm still working on getting the speed up - not that anything has failed on me just worried my hotend won't keep up and haven't tested max volumetric flow yet
I tried .8 nozzle for a while, but my vanilla hot end just can't keep up at higher speed.
I could not get a 0.6 to stop oozing and stringing with petg and pla. Just couldn't so switched back to 0.4. Dragon hot end w. Bowden tube after titan extruder.
can't believe it - I was stringing and clogging with 0.4 (likely trouble with retraction but tuned to hell and back) but running same parts at 0.8 (granted not detailed, but functional big parts) without stringing, same retraction settings, and 40% print time it's wild
I wonder if it's the particular blend? I was using PLA+ and PETG both from ESun.