this post was submitted on 11 Feb 2024
9 points (90.9% liked)

3DPrinting

15605 readers
205 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

My prints get very good adhesion to the bed, especially when doing prints with large adhesion areas. So good, that after the print is done, I actually have to wet the surface with alcohol and put it in the freezer for it to let go! (edit: I print with PLA)

My question is, if the adhesion could be a bit less violent, if I lower or increase the bed temperature? I have an ender 3 v2 with the original glass bed (it has some black layer on top of the glass).

I know that there are tons of alternative beds that I could buy, but I'd rather keep this bed if I can counter the too strong adhesion

you are viewing a single comment's thread
view the rest of the comments
[–] cosmicrookie 1 points 9 months ago (3 children)

So you use glue to make adhesion worse? That's very interesting!

[–] [email protected] 3 points 9 months ago

Yup. My kid found the idea hilarious when I explained why I’d swiped a washable glue stick from the arts and crafts box.

It hangs on well, but also makes removal easier.

[–] [email protected] 2 points 9 months ago (2 children)

Adhesion can be better, but it also acts as a release agent. If you are printing PETG on glass always use glue, for PLA it shouldnt be needed.

[–] [email protected] 1 points 9 months ago

glue or hairspray

[–] cosmicrookie 1 points 9 months ago (1 children)

I am in deed printing with Pla but it sticks waaaay too well onto the surface

[–] [email protected] 2 points 9 months ago

In my experience PLA just pops off the clean glass when cooled to room temp (holds extremely well if bed is at 45C or more). I have some tips, but only to improve adhesion xD You can maybe try less squish on the first layer (lower flow rate or increase nozzle distance a bit) or just use thin layer of glue. Too low or too high bed temp can ruin bed adhesion, but feels like wrong approach imo, still worth a try

[–] [email protected] 2 points 9 months ago

I use the washable gluesticks for my polycarbonate prints. I just put PC prints under warm water for a few minutes and they pop right off. Gluesticks generally reduce bed adhesion though IME, so it's a fine line to walk; I never use gluesticks with PETG for example because then the parts don't stick to the bed enough.