this post was submitted on 22 Jun 2023
65 points (100.0% liked)

3DPrinting

16071 readers
87 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 
you are viewing a single comment's thread
view the rest of the comments
[–] mattaw 1 points 2 years ago* (last edited 2 years ago) (2 children)

I could not get a 0.6 to stop oozing and stringing with petg and pla. Just couldn't so switched back to 0.4. Dragon hot end w. Bowden tube after titan extruder.

[–] jtablerd 1 points 2 years ago (1 children)

can't believe it - I was stringing and clogging with 0.4 (likely trouble with retraction but tuned to hell and back) but running same parts at 0.8 (granted not detailed, but functional big parts) without stringing, same retraction settings, and 40% print time it's wild

[–] mattaw 1 points 2 years ago

I wonder if it's the particular blend? I was using PLA+ and PETG both from ESun.