this post was submitted on 28 Jul 2023
18 points (100.0% liked)

3DPrinting

15606 readers
242 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Title sums it up, any other tips about PETG appreciated though.

you are viewing a single comment's thread
view the rest of the comments
[–] Zeth 2 points 1 year ago (1 children)

My goto on a glass bed was blue painters tape applied with a spatula or flat tool. I discovered that the natural oils off my fingers transfered to the painters tape when applying making the first layer fail to stick every time.

[–] [email protected] 1 points 1 year ago

PETG is a diva. If something's not perfect, it refuses to print. My CR-10 had the infamous first version of the Creality bed springs, and vibrations would cause enough movement of the tramming springs, the print would fail. Even watching it put down a perfect line of filament, it would move and fail during the first layer on a larger print. My problems mostly went away after upgrading bed springs.

Also, I live in a swampy area, I have to print PETG out of a heated dryer set to 55 degrees all the time. That took care of almost all of the other problems.

PETG is softer than PLA, so the extruder "bites" it differently. Calibrating my e-steps for PETG was the final key to printing great PETG parts.

I still think ASA is easier for me to print than PETG.