Hey all, so this is the biggest thing I've tried to print. I'm using PETG. I'm getting a lot of repetitive bands of underextrusion that seem to stack up and get worse as the print progresses.

What do you think is causing this? Is this just an inherent thing in the way an Ender 3 works by moving the bed?

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 1 points 1 year ago* (last edited 1 year ago)

The "struggle" is having a PTFE lined hotend which have a maximum temperature limit between 200 to 250C depending on what pets you have, and a thermistor that maxes out at 285C - both which are well within the PETG temperatures though. Ignore both of those and the heater actually has enough oomph to cause the aluminium heater block to melt into a puddle.