this post was submitted on 05 Jan 2024
336 points (99.1% liked)
Asklemmy
43945 readers
37 users here now
A loosely moderated place to ask open-ended questions
Search asklemmy ๐
If your post meets the following criteria, it's welcome here!
- Open-ended question
- Not offensive: at this point, we do not have the bandwidth to moderate overtly political discussions. Assume best intent and be excellent to each other.
- Not regarding using or support for Lemmy: context, see the list of support communities and tools for finding communities below
- Not ad nauseam inducing: please make sure it is a question that would be new to most members
- An actual topic of discussion
Looking for support?
Looking for a community?
- Lemmyverse: community search
- sub.rehab: maps old subreddits to fediverse options, marks official as such
- [email protected]: a community for finding communities
~Icon~ ~by~ ~@Double_[email protected]~
founded 5 years ago
MODERATORS
you are viewing a single comment's thread
view the rest of the comments
view the rest of the comments
I try not to use a lot of plastic wrap, but sometimes it's the right tool for the job. I will always spring for the good stuff, generic is basically useless and you waste way more for inferior performance.
I work as QA in packaging and it turns out that it's super important for a manufacturer to follow every little specification for consistency. There's some seriously small details that make a big difference.
Oh I bet the line between "won't stick to anything" and "immediately turns into a useless wad" is razor thin.
We use dimethyl sulfoxide to test for saran coating. We don't really make cling wrap where I work though. That's usually for anti fog or sealing layers.